40699146 0 RPU 70 TDS.pdf

DOC #103213 REV D

CarbonResin RPU 70

TECHNICAL DATA SHEET, LAST UPDATED 08/14/2017

RPU 70

RPU 70 is a tough, heat resistant material that is a good choice for parts requiring

strength, toughness, and moderate heat resistance.


Tensile Properties ASTM D638, Type V 10 mm/min
Tensile Modulus
Ultimate Tensile Strength
Tensile Strength at Yield
Elongation at Break
Flexural Properties ASTM D790
Flexural Strength
Flexural Modulus
Impact Properties
Notched Izod (Machined), 23 °C, ASTM D256
Notched Izod (Machined), -30 °C, ASTM D256
Unnotched Izod, ASTM D4812
Notched Charpy, ISO 179-1/1eA
Thermal Properties
Heat Deflection Temperature @ 0.455 MPa/66 psi, ASTM D648
Heat Deflection Temperature @ 1.82 MPa/264 psi, ASTM D648
Coefficient of Thermal Expansion (-40, 40 °C), ASTM E831
Flammability, UL 94 (1.5 mm)
General Properties
Hardness, ASTM D2240
Density, ASTM D792
Density (liquid resin)
Water Absorption, 23 °C, 24 hours, ASTM D570
Water Absorption, 23 °C, long term, ASTM D570
Metric U.S.
1900±200MPa 290±30ksi
45±2MPa 6.5±0.3ksi
45±2MPa 6.5±0.3ksi
100±20%
62±9MPa 9.0±1.3ksi
1800±300MPa 261±40ksi
22±1J/m 0.41±0.02ft-lb/in
19±4J/m 0.36±0.07ft-lb/in
530±30J/m 9.9±0.5ft-lb/in
1.83±0.15kJ/m² 0.871±0.071ft-lb/in²
70℃ 160℉
55℃ 130℉
96ppm/℃ 53ppm/℉
HB
80,ShoreD
1.076g/cm³
1.01g/cm³
0.31%
1.01%

NOTES— Results in this data sheet are representative of specific sample generation and testing processes and may vary if the established protocols are not followed. Contact Carbon for the specific process used to generate the test samples to determine each of these values. Tensile and flexural data are average ± 1 standard deviation from 16 specimens; impact data used 10 specimens. The U.S. values are converted from Metric measurements and are for reference only.